Sizes: 5nm, 10nm, 15nm and 20nm gold nanoparticles
Surface Composition: 5nm & 10nm - tannic acid, 15nm & 20nm - citrate
Quantity: 20ml of each size at OD=1
Buffer: Supplied in 0.1mM phosphate buffered saline
Four sizes of unconjugated gold nanoparticles spanning the lower size range from 5nm to 20nm combined in a convenient kit for testing of optimal size and suitability during your protocol development. Ideal for use in electron microscopy and blotting applications.
Properties
These gold nanoparticles have a narrow size distribution (CV of less than 12%), high protein binding capability and are more than 95% spherical. Low batch to batch variability (+/- 2nm) assures you as a customer always end up with a product within the specified size range ordered.
Storage
Store product away from direct sunlight at 4-25°C. Lower temperature prolongs the shelf life of the product.
Do Not Freeze
When stored as specified the product is stable for at least six months.